Fatigue properties of as-welded and post-weld-treated high-strength steel joints: The influence of constant and variable amplitude loads

Publikation: Bidrag til tidsskrift/Konferencebidrag i tidsskrift /Bidrag til avisTidsskriftartikelForskningpeer review

  • Halid Can Yıldırım
  • Heikki Remes, Aalto University
  • ,
  • Alain Nussbaumer, Swiss Federal Institute of Technology Lausanne

In HSS welded structures, HFMI allows fatigue strength improvement factors by inducing compressive residual stresses, cold-worked surface region and modifying the weld toe shape. According to the literature, the factors are proposed based on failures at CAL and also checked with a limited dataset at VAL, the latter being more realistic of service loadings. Therefore, this paper investigates the behaviour of HFMI welds at CAL and VAL for R = −0.43. Studies are also performed at the microstructural level for locating the crack initiation and hardness. Fatigue damage sums are evaluated and discussed with the recommended values in the literature.

OriginalsprogEngelsk
Artikelnummer105687
TidsskriftInternational Journal of Fatigue
Vol/bind138
ISSN0142-1123
DOI
StatusUdgivet - sep. 2020

Se relationer på Aarhus Universitet Citationsformater

ID: 189811232